Data

Static Shielding Bag Specifications

 

Material: Buried Metal

 

Construction: Anti-Static Outer Surface, Polyester, Metal, Polyethylene, Anti-Static Inner Coating

 

Physical Properties

Test Method

Specification

Thickness

TCI #001

3.0 mil +/- 5%

Puncture Resistance

FTMS 101C method 2065

12 lbs.

Yield

TCI #002

9300 sq in / lb

Tensile Strength

ASTM D-882-67

MD>16 lbs./in

TD> 15 lbs./in

Mullen Burst

ASTM D-774

>100 psi

Seal Strength

ASTM 188-94

>12 lbs./in

Ply Bond

ASTM D - 1876-95

MD>2.0 lbs.p/in

TD>2.5 lbs./in

Optical Density

0.35 - 0.45

Tear Intiation

ASTM D-1004

MD>2.0 lbs./in

TD>2.5 lbs./in

MVTR

ASTM F-1249

.35 gms nominal

Haze

ASTM D-1003

4%

Transparency

ASTM D-1003

40%

Heat Seal

375° F 0.5 sec. 60 psi

Blocking

None

Electrical Properties

Test Method

Specification

Surface Resistivity

EOS/ESD - S11.11.1993

PE<10 OHMS

PEY<10 OHMS

Electrostatic Decay

FTMS 101 method 4046

.01 sec.

Capacitance Probe

EIA - 541

<30 volts difference

Metal Layer

ETS-803 at 12% RH

<100